6063 Wood Grain Anodized Aluminum Extrusion Profiles for Booth Exhibition Stand-1
Aluminum extrusion window frame Processing:
1.Raw material purchase
2.Extruding aluminum extrusion window frame
3.Put in semi-finished products warehouse
4.after the acid and alkali chemical reation
5.Natural anodized
6.Air driving
7.Packaging
8.Saved in finished products warehouse
Feeding:
(1) the contact surface of the hanger should be grinded clean before the material is on the material, and the formula is calculated according to the standard number. The calculation formula: the number of the material = standard current standard current density and the area of the single section section
(2)The principle of considering the number of supports on the shelf
(3) Calculation of oxidation time: oxidation time (T) = film thickness K. Current density K is the electrolytic constant. Take 0.26 - 0.32, t unit is minute.
(4) The upper row must be placed on the basis of the number of sections specified in the section area and the upper row number table.
(5)In order to facilitate drainage and exhaust, the upper row should be tilted and the inclination should be 5 degrees.











share to: